#583. Tempering Liquid

- By Formula pot

Ingredients

  • Refer procedure

Procedure:

To 6 quarts of soft water put in corrosive sublimate, 1 oz.; common salt, 2 handfuls; when dissolved it is ready for use. The first gives toughness to the steel, while the latter gives the hardness. Be careful with this preparation, as it is a dangerous poison.